{"id":1395,"date":"2026-08-26T09:06:50","date_gmt":"2026-08-26T01:06:50","guid":{"rendered":"https:\/\/sheeonpulp.com\/?post_type=news&#038;p=1395"},"modified":"2026-08-26T09:06:50","modified_gmt":"2026-08-26T01:06:50","slug":"bagasse-pulp-complete-guide-for-buyers","status":"publish","type":"news","link":"https:\/\/sheeonpulp.com\/de\/nachrichten\/bagasse-pulp-complete-guide-for-buyers\/","title":{"rendered":"Bagasse Pulp: Complete Guide for Buyers"},"content":{"rendered":"<p>Sheeon Pulp Technical Team | Technical Content Team | Published: August 26, 2026<\/p>\n<p><span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/de\/kategorie\/bagasse-zellstoff\/\">Bagasse-Zellstoff<\/a><\/strong><\/span> is fiber pulp made from sugarcane bagasse, the fibrous residue left after juice extraction, processed into either a bleached grade (brightness &gt;80%) for tableware and printing applications or an unbleached grade (brightness 40\u201343%) for bulk packaging and industrial uses.<\/p>\n<h2>What Bagasse Pulp Is and Where It Comes From<\/h2>\n<p>Bagasse is a byproduct of sugarcane processing \u2014 the crushed stalk material remaining after sugar mills extract the juice. Rather than being discarded or burned as fuel, bagasse can be pulped into fiber suitable for paper, packaging and molded fiber products, giving buyers a non-wood alternative to conventional pulp sourcing. This matters most to manufacturers looking to diversify fiber supply away from wood pulp, either for cost, sustainability positioning or regional sourcing reasons.<\/p>\n<p>Sheeon supplies bagasse pulp across more than 50 countries, with named long-term markets in Germany, Belgium, Spain, France and the Netherlands. That geographic spread reflects a fiber source with established international demand, not a niche or regional-only material.<\/p>\n<h2>Bleached vs. Unbleached: The Core Decision<\/h2>\n<p>The first sourcing decision for any bagasse pulp buyer is grade. Bleached and <span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/de\/ungebleichter-bagasse-zellstoff\/\">ungebleichter Bagasse-Zellstoff<\/a> <\/strong><\/span>differ substantially \u2014 not just in color, but in processing, beating degree and typical end use.<\/p>\n<table border=\"1\">\n<tbody>\n<tr>\n<td width=\"165\"><strong><b>Parameter<\/b><\/strong><\/td>\n<td width=\"142\"><strong><b>Gebleichter Bagasse-Zellstoff<\/b><\/strong><\/td>\n<td><strong><b>Ungebleichter Bagasse-Zellstoff<\/b><\/strong><\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Helligkeit<\/td>\n<td width=\"142\">&gt;80%<\/td>\n<td>40\u201343%<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Schmutzmenge, 0,3\u20135,0 mm\u00b2<\/td>\n<td width=\"142\">&lt;35 mm\u00b2\/500 g<\/td>\n<td>&lt;40 mm\u00b2\/500 g<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Schmutzmenge, &gt;5,0 mm\u00b2<\/td>\n<td width=\"142\">Keine<\/td>\n<td>Keine<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Zugfestigkeitsindex<\/td>\n<td width=\"142\">&gt;55 N\u00b7m\/g<\/td>\n<td>\u2014 (not disclosed)<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Pr\u00fcgelgrad<\/td>\n<td width=\"142\">22\u00b0 s\u00fcdlicher Breite<\/td>\n<td>18\u00b0 s\u00fcdlicher Breite<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Luftfeuchtigkeit<\/td>\n<td width=\"142\">&lt;15%<\/td>\n<td>14 \u00b1 21 TP3T<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">pH-Wert<\/td>\n<td width=\"142\">6,5\u20138,0<\/td>\n<td>&lt;8,0<\/td>\n<\/tr>\n<tr>\n<td width=\"165\">Sheet\/bale format<\/td>\n<td width=\"142\">700 \u00d7 800 mm sheet<\/td>\n<td>700 \u00d7 800 \u00d7 600 mm bale, 250 kg ADMT<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>The unbleached grade&#8217;s lower beating degree (18\u00b0SR against 22\u00b0SR) means less fiber refining has already taken place, which typically translates into a lower per-ton cost and suits applications where surface whiteness isn&#8217;t a requirement \u2014 cushioning layers, non-visible packaging components, or as a blend input for mills doing their own further processing.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"\" src=\"https:\/\/sheeonpulp.com\/wp-content\/uploads\/2026\/03\/Bleached-Bagasse-pulp-3.webp\" alt=\"Gebleichter Bagasse-Zellstoff\" width=\"566\" height=\"566\" \/><\/p>\n<h2>Full Specification: Bleached Bagasse Pulp<\/h2>\n<p>For manufacturers sourcing tableware-grade or printing-grade pulp, the complete published specification is:<\/p>\n<p>&nbsp;<\/p>\n<table border=\"1\">\n<tbody>\n<tr>\n<td><strong><b>Parameter<\/b><\/strong><\/td>\n<td><strong><b>Wert<\/b><\/strong><\/td>\n<td><strong><b>Pr\u00fcfverfahren<\/b><\/strong><\/td>\n<\/tr>\n<tr>\n<td>Helligkeit<\/td>\n<td>&gt;80%<\/td>\n<td>GB\/T 8940.2<\/td>\n<\/tr>\n<tr>\n<td>Schmutzmenge, 0,3\u20135,0 mm\u00b2<\/td>\n<td>&lt;35 mm\u00b2\/500 g<\/td>\n<td>GB\/T 7974<\/td>\n<\/tr>\n<tr>\n<td>Zugfestigkeitsindex<\/td>\n<td>&gt;55 N\u00b7m\/g<\/td>\n<td>GB\/T 10740-1989<\/td>\n<\/tr>\n<tr>\n<td>Tr\u00e4nenindex<\/td>\n<td>&gt;5,0 mN\u00b7m\u00b2\/g<\/td>\n<td>QB\/T 3704<\/td>\n<\/tr>\n<tr>\n<td>Burst-Index<\/td>\n<td>&gt;4,0 kPa\u00b7m\u00b2\/g<\/td>\n<td>GB\/T 1548<\/td>\n<\/tr>\n<tr>\n<td>Viskosit\u00e4t<\/td>\n<td>&gt;550 cm\u00b3\/g<\/td>\n<td>GB\/T 742<\/td>\n<\/tr>\n<tr>\n<td>Faser-Nassgewicht<\/td>\n<td>&gt;1,7 g<\/td>\n<td>GB\/T 8944.1<\/td>\n<\/tr>\n<tr>\n<td>Esche<\/td>\n<td>&lt;0,7%<\/td>\n<td>GB\/T 3332-2004<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<h2>Full Specification: Unbleached Bagasse Pulp<\/h2>\n<table border=\"1\">\n<tbody>\n<tr>\n<td><strong><b>Parameter<\/b><\/strong><\/td>\n<td><strong><b>Wert<\/b><\/strong><\/td>\n<\/tr>\n<tr>\n<td>Helligkeit<\/td>\n<td>40\u201343%<\/td>\n<\/tr>\n<tr>\n<td>Schmutzmenge, 0,3\u20135,0 mm\u00b2<\/td>\n<td>&lt;40 mm\u00b2\/500 g<\/td>\n<\/tr>\n<tr>\n<td>Fl\u00e4chengewicht<\/td>\n<td>500\u2013530 g\/m\u00b2<\/td>\n<\/tr>\n<tr>\n<td>Ballengewicht<\/td>\n<td>250 kg ADMT<\/td>\n<\/tr>\n<tr>\n<td>Luftfeuchtigkeit<\/td>\n<td>14 \u00b1 21 TP3T<\/td>\n<\/tr>\n<tr>\n<td>pH-Wert<\/td>\n<td>&lt;8,0<\/td>\n<\/tr>\n<tr>\n<td>Pr\u00fcgelgrad<\/td>\n<td>18\u00b0 s\u00fcdlicher Breite<\/td>\n<\/tr>\n<\/tbody>\n<\/table>\n<p>Note the gap here: tensile, tear and burst index figures are published for the bleached grade but not disclosed for unbleached on the reviewed pages. Mills evaluating <span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/de\/ungebleichter-bagasse-zellstoff\/\">ungebleichter Bagasse-Zellstoff<\/a><\/strong><\/span> for strength-dependent applications should request these figures directly rather than assume parity with the bleached grade.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"\" src=\"https:\/\/sheeonpulp.com\/wp-content\/uploads\/2026\/03\/Unbleached-Bagasse-Pulp-3.webp\" alt=\"Ungebleichter Bagasse-Zellstoff\" width=\"562\" height=\"562\" \/><\/p>\n<h2>Applications by Fiber Grade<\/h2>\n<p>Molded fiber tableware. <span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/de\/gebleichter-bagasse-zellstoff\/\">Gebleichter Bagasse-Zellstoff<\/a><\/strong><\/span>&#8216;s brightness above 80% avoids a secondary whitening step, and its tensile index above 55 N\u00b7m\/g and burst index above 4.0 kPa\u00b7m\u00b2\/g support the pressing and forming process without excessive rim cracking.<\/p>\n<p>Industrial and bulk packaging. Unbleached bagasse pulp&#8217;s lower processing cost and 250 kg ADMT bale format suit cushioning, trays and non-visible packaging layers where whiteness adds no functional value.<\/p>\n<p>Printing and specialty paper. Bleached bagasse pulp&#8217;s ash content under 0.7% and moisture under 15% keep mineral residue and drying variability low, relevant for mills blending it into printing-grade furnish.<\/p>\n<p>Paper mill furnish blending. Mills incorporating bagasse pulp into a broader fiber mix weigh tensile index, tear index and viscosity more heavily than sheet format, since these determine compatibility with existing wood or other alternative-fiber stock in the blend.<\/p>\n<h2>An Edge Case Buyers Often Miss: Grade Mismatch in Blended Furnish<\/h2>\n<p>One issue that surfaces after order confirmation rather than before it: mills sometimes order bleached bagasse pulp assuming it will behave identically to unbleached stock once re-pulped into a blend, since both start from the same raw material. It doesn&#8217;t. The higher beating degree on the bleached grade (22\u00b0SR against 18\u00b0SR) means it arrives already more refined, which changes how it responds in a mill&#8217;s own beater or refiner compared to unbleached stock. Running both grades through an identical downstream process without adjusting refining time can produce inconsistent furnish results \u2014 this is a processing variable to test in a trial run, not something to assume matches across grades.<\/p>\n<h2>Certification Claims: What&#8217;s Published and What Isn&#8217;t<\/h2>\n<p><span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/de\/gebleichter-bagasse-zellstoff\/\">Bagasse-Zellstoff<\/a> <\/strong><\/span>product pages carry CE, FDA-related food-contact and SGS verification claims. None of the reviewed pages disclose certificate numbers, issuing bodies or validity dates for these claims at the individual product level.<\/p>\n<p>This is worth taking seriously for tableware and food-packaging buyers specifically. CE marking indicates conformity with applicable EU harmonisation legislation \u2014 it is not, on its own, a food-contact certificate. Food-contact material compliance in the EU market is governed separately under Regulation (EC) No 1935\/2004. Before finalizing an order for food-contact applications, request the specific test report or declaration of conformity that matches the exact bagasse pulp grade and lot \u2014 a website claim is a starting point for the conversation, not the documentation itself.<\/p>\n<p><img loading=\"lazy\" decoding=\"async\" class=\"\" src=\"https:\/\/sheeonpulp.com\/wp-content\/uploads\/2026\/03\/Bleached-Bagasse-pulp-2.webp\" alt=\"Gebleichter Bagasse-Zellstoff\" width=\"582\" height=\"582\" \/><\/p>\n<h2>Preisbestimmende Faktoren<\/h2>\n<p>No fixed price list is published for bagasse pulp. Pricing depends on grade (bleached or unbleached), specification, order volume, packaging and delivery requirements. Buyers should expect to submit tonnage, grade and delivery terms to receive a quote rather than compare a published per-ton figure across suppliers \u2014 this is standard for the category rather than a gap specific to any one supplier.<\/p>\n<h2>Sourcing Checklist Before Placing an Order<\/h2>\n<ul>\n<li>Confirm which grade \u2014 bleached or unbleached \u2014 matches your end application, not just your target price point.<\/li>\n<li>Request tensile, tear and burst index figures directly if sourcing unbleached grade for a strength-sensitive application, since these aren&#8217;t published on the reviewed pages.<\/li>\n<li>Match any CE, FDA or SGS claim to an actual certificate or test report before relying on it for food-contact procurement decisions.<\/li>\n<li>Confirm basis weight and bale dimensions for your specific grade \u2014 published figures differ between bleached and unbleached, and bleached-grade basis weight isn&#8217;t disclosed.<\/li>\n<li>Submit exact tonnage and delivery terms for a price quote; published price ranges don&#8217;t exist for this category.<\/li>\n<\/ul>\n<h2>Vorteile und Kompromisse<\/h2>\n<p>What bagasse pulp offers buyers diversifying fiber supply:<\/p>\n<ul>\n<li>A non-wood fiber source with published specs comparable in structure to conventional pulp documentation (brightness, tensile, tear, burst all cited against named test methods).<\/li>\n<li>Two distinct grades covering both premium white-surface applications and lower-cost bulk packaging needs from a single fiber source.<\/li>\n<li>Established international supply history \u2014 <span style=\"color: #ff6600;\"><strong><a style=\"color: #ff6600;\" href=\"https:\/\/sheeonpulp.com\/index.php\/service\/\">Sheeon<\/a> <\/strong><\/span>reports commercial coverage across more than 50 countries, with specific long-term development in the European market.<\/li>\n<\/ul>\n<p>What buyers should factor in before switching sourcing:<\/p>\n<ul>\n<li>Certificate numbers for stated compliance claims aren&#8217;t published, adding a verification step to food-contact procurement that a wood-pulp supplier with disclosed certificates might not require.<\/li>\n<li>Strength-index figures (tensile, tear, burst) are incomplete for the unbleached grade, meaning strength-dependent buyers need supplier follow-up before finalizing a spec.<\/li>\n<li>No published price range means sourcing comparisons across suppliers require direct quote requests rather than published-rate comparison.<\/li>\n<\/ul>\n<h2>FAQ<\/h2>\n<h3>Q: What&#8217;s the main difference between bleached and unbleached bagasse pulp?<\/h3>\n<p>A: Brightness is the most visible difference \u2014 &gt;80% for bleached against 40\u201343% for unbleached \u2014 but beating degree (22\u00b0SR vs. 18\u00b0SR) and typical end use (tableware\/printing vs. bulk packaging) matter just as much for a sourcing decision.<\/p>\n<h3>Q: Is bagasse pulp certified for food contact?<\/h3>\n<p>A: Sheeon&#8217;s product pages carry FDA-related food-contact and CE claims, but certificate numbers and issuing bodies aren&#8217;t disclosed. Request the specific documentation matched to your grade and lot before relying on the claim for a food-contact order.<\/p>\n<h3>Q: What tensile or tear strength does unbleached bagasse pulp have?<\/h3>\n<p>A: These figures aren&#8217;t published for the unbleached grade on the reviewed pages. Buyers needing strength data for unbleached stock should request it directly from the supplier.<\/p>\n<h3>Q: Can I get a fixed price for bagasse pulp?<\/h3>\n<p>A: No published price list exists. Pricing depends on grade, specification, order volume, packaging and delivery terms, confirmed through a direct quote request.<\/p>","protected":false},"excerpt":{"rendered":"<p>Bagasse pulp is fiber pulp made from sugarcane bagasse, the fibrous residue left after juice extraction, processed into either a bleached grade (brightness >80%) for tableware and printing applications or an unbleached grade (brightness 40\u201343%) for bulk packaging and industrial uses.<\/p>","protected":false},"featured_media":1289,"comment_status":"closed","ping_status":"closed","template":"","class_list":["post-1395","news","type-news","status-publish","has-post-thumbnail","hentry"],"acf":[],"_links":{"self":[{"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/news\/1395","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/news"}],"about":[{"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/types\/news"}],"replies":[{"embeddable":true,"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/comments?post=1395"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/media\/1289"}],"wp:attachment":[{"href":"https:\/\/sheeonpulp.com\/de\/wp-json\/wp\/v2\/media?parent=1395"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}